Hi All,
I have an ore stockpile which I assayed and it contains:
843ppm Ag
5.2% Zn
1.3% Cu
9000ppm Sb
1520 Pb
2.7% As
5% Sulphur
I haven't tried roasting yet and have tried smelting the concentrate using fluxes. The first attempt I added an Iron rod to the crucible to help reduce the sulphur...
Hello my name is Rod Triplett and have owned several pawnshops over the last 32 years. I have always just sent my scrap to refiners and gotten paid. Now I am more interested in smelting my own and possibly getting into the refining area. So just learning, making mistakes and hoping to get some...