    Recovery of Iridium from Iridium coated Titanium Mesh.

    I have titanium anodes which are coated with iridium oxide as far as I have researched. I have cut the mesh into small pieces and thrown it in hot concentrated HCL. This resulted in the coating being removed and the coating settled at the bottom as a black powder. I filtered this powder and...