I have been refining for about 12 months using Nitric at 70%. I found a local supplier with 67% at a good price. Is there any reason why I could not use 67%? It may be a stupid question, but with chemistry, sometimes the logical obvious is wrong....
Excellent, thank youThe 67% will work fine for refining.