• Please join our new sister site dedicated to discussion of gold, silver, platinum, copper and palladium bar, coin, jewelry collecting/investing/storing/selling/buying. It would be greatly appreciated if you joined and help add a few new topics for new people to engage in.

    Bullion.Forum

Chemical Aqua Regia Completion

Gold Refining Forum

Help Support Gold Refining Forum:

This site may earn a commission from merchant affiliate links, including eBay, Amazon, and others.

IThinkSilver

New member
Joined
Feb 27, 2025
Messages
1
Location
Ramah, NM 87321
I used AR to process some RAM chips. Since I didn’t know how much gold was there, I added aziotropic nitric acid drop by drop. In total I added about 10 drops, less than 1/2 ml. I filtered the AR and ended up with about 1000 ml after hydration with distilled water. I took a 100 ml sample of the AR and tried to precipitate with SMB but nothing happened except solution turned colorless. Assuming there was excess nitric, I added about 6 spoons of clean gold foils until no more would dissolve. Again, I took 100 ml sample and same results as first try. Upon consulting Hoke, I boiled the AR down to about 150 ml of thick brownish golden liquid. Then, I added HCL to react with any remaining nitric. So here I am now at this point, not sure how to proceed. Solution is in 2 L beaker. I have seen some recommend using sulfamic acid to correct pH I think. What steps are left to get the AR solution ready for SMB?
 
I used AR to process some RAM chips. Since I didn’t know how much gold was there, I added aziotropic nitric acid drop by drop. In total I added about 10 drops, less than 1/2 ml. I filtered the AR and ended up with about 1000 ml after hydration with distilled water. I took a 100 ml sample of the AR and tried to precipitate with SMB but nothing happened except solution turned colorless. Assuming there was excess nitric, I added about 6 spoons of clean gold foils until no more would dissolve. Again, I took 100 ml sample and same results as first try. Upon consulting Hoke, I boiled the AR down to about 150 ml of thick brownish golden liquid. Then, I added HCL to react with any remaining nitric. So here I am now at this point, not sure how to proceed. Solution is in 2 L beaker. I have seen some recommend using sulfamic acid to correct pH I think. What steps are left to get the AR solution ready for SMB?
Welcome.
Have you already read Hokes book?

If not, it's here with other important links to study:

We ask our new members to do 3 things.
1. Read C.M. Hokes book on refining jewelers scrap, it gives an easy introduction to the most important chemistry regarding refining.
It is free here on the forum: https://goldrefiningforum.com/phpBB3/viewtopic.php?f=54&t=19798
2. Then read the safety section of the forum: https://goldrefiningforum.com/threads/library-index-thread.22351/post-233795
3. And then read about "Dealing with waste" in the forum: https://goldrefiningforum.com/threads/library-index-thread.22351/post-233794

Suggested reading:
https://goldrefiningforum.com/forums/the-library.101/
https://goldrefiningforum.com/threads/when-in-doubt-cement-it-out.30236/
https://goldrefiningforum.com/threa...le-read-this-before-you-post-about-ore.35743/

Video section: https://goldrefiningforum.com/threa...our-visual-learning-members.35185/post-379931

List of abbreviations: https://goldrefiningforum.com/threads/a-glossary-of-common-terms.21242/post-219169

Forum rules is here.
https://goldrefiningforum.com/threads/gold-refining-forum-rules.31182/
 
Last edited:
I used AR to process some RAM chips. Since I didn’t know how much gold was there, I added aziotropic nitric acid drop by drop. In total I added about 10 drops, less than 1/2 ml. I filtered the AR and ended up with about 1000 ml after hydration with distilled water. I took a 100 ml sample of the AR and tried to precipitate with SMB but nothing happened except solution turned colorless. Assuming there was excess nitric, I added about 6 spoons of clean gold foils until no more would dissolve. Again, I took 100 ml sample and same results as first try. Upon consulting Hoke, I boiled the AR down to about 150 ml of thick brownish golden liquid. Then, I added HCL to react with any remaining nitric. So here I am now at this point, not sure how to proceed. Solution is in 2 L beaker. I have seen some recommend using sulfamic acid to correct pH I think. What steps are left to get the AR solution ready for SMB?
I'd like some clarification on your material.
Ram Chips, means in this setting the whole stick or the only the chips?
How many was there?

AR is not suitable for PCB stripping.
 