R rodshanz Member Joined Jun 1, 2008 Messages 19 Location maine Aug 27, 2008 #1 hello i ben working on what i did roung. I put to much clorox how do i get it out its ben a week and it rilly has alot in
hello i ben working on what i did roung. I put to much clorox how do i get it out its ben a week and it rilly has alot in
Noxx Well-known member Joined Feb 24, 2007 Messages 3,365 Location Quebec, Canada Aug 27, 2008 #2 Ok if I understand correctly, you say that you added too much chlorox. You can't get the Chlorox out (why would you do so ?) but you can get the chlorine out (Cl) by heating the solution a bit for a few hours.
Ok if I understand correctly, you say that you added too much chlorox. You can't get the Chlorox out (why would you do so ?) but you can get the chlorine out (Cl) by heating the solution a bit for a few hours.
Rag and Bone Well-known member Joined Apr 1, 2008 Messages 612 Location Upper Midwest Aug 27, 2008 #3 Gently boil it on a hot plate. It will put off lots of chlorine fumes so do it outside somewhere safe.
Gently boil it on a hot plate. It will put off lots of chlorine fumes so do it outside somewhere safe.