GuyGuyGuythe1st
Active member
I just wanted to share some silver single refined. Still has to go through an electro cell.
This is the biggest lot I’ve ever processed. It’s the second time I’ve ever process a large batch.
Starting Materials: 7.5 Kg Silver Foils
Net Yield: About 5 KG
This is the biggest lot I’ve ever processed. It’s the second time I’ve ever process a large batch.
Starting Materials: 7.5 Kg Silver Foils
Net Yield: About 5 KG