• Please join our new sister site dedicated to discussion of gold, silver, platinum, copper and palladium bar, coin, jewelry collecting/investing/storing/selling/buying. It would be greatly appreciated if you joined and help add a few new topics for new people to engage in.

    Bullion.Forum

Non-Chemical Can you use thermite to get Platinum?

Gold Refining Forum

Help Support Gold Refining Forum:

This site may earn a commission from merchant affiliate links, including eBay, Amazon, and others.
I've burned holes in steel plate with the Calcium Sulfate/Aluminum mix. In the Trade, it's called Alice Mix. It will also throw chunks of burning metal for quite a distance. It's a good way to burn your house down. Any moisture will cause a steam explosion, which will throw burning metal in all directions.
 
Thanks for responding guys. I've looked through the link you posted Steve, and couldn't anything on Platinum. Even still, would it be possible to separate platiunum by adding ground up catalytic converters to a high energy thermite mix?

Thanks again
 
Witness said:
Thanks for responding guys. I've looked through the link you posted Steve, and couldn't anything on Platinum. Even still, would it be possible to separate platiunum by adding ground up catalytic converters to a high energy thermite mix?

Thanks again

I don't think so. What you would get is Pt dispersed in a mix of Iron and Aluminum Oxide.
 
Irons said:
I've burned holes in steel plate with the Calcium Sulfate/Aluminum mix. In the Trade, it's called Alice Mix. It will also throw chunks of burning metal for quite a distance. It's a good way to burn your house down. Any moisture will cause a steam explosion, which will throw burning metal in all directions.

Well damn... now I GOTTA try this! My property looks like Mad Max's Thunderdome anyhow so if something burns down, it's an improvement.
 
Funny you should mention that, Witness. One document I read had the honeycomb wash getting attacked by magnesium vapour inside a high temperature retort. Kind of like a very slow motion thermite.
 
Witness,

There is no need to use thermite to get Pt from CC honeycomb. It can
be melted other ways that are industry proven and can be done at fairly
small scale. I have built a system that does this that can process 0.25 ton/day
and am planning to build a 5-10 ton/day. The process uses an electrical arc
furnace system to smelt the PGM from the aluminum silicates.

PS
 
Lou,

Were you directing the response my way?
I've got some good photos of melting AC I can share.
Just let me know sir.

PS
 
plasmasmelter said:
Lou,
Were you directing the response my way?
I've got some good photos of melting AC I can share.
PS

I'm sure he was, and if not, I would certainly be interested in seeing them!
 
seem that if a cheap enough source of aluminum powder could be found this would be a way to recover the base metals from processing electronic scrap. I know that if I could take
nuggets of metal that the junk yard could test with their gun thing, they will pay based on the print out. I already get that with recovered copper bars that I cast.

Nickel, cobalt, and tin are fairly valuable metals.

Jim
 
plasmasmelter said:
Witness,

There is no need to use thermite to get Pt from CC honeycomb. It can
be melted other ways that are industry proven and can be done at fairly
small scale. I have built a system that does this that can process 0.25 ton/day
and am planning to build a 5-10 ton/day. The process uses an electrical arc
furnace system to smelt the PGM from the aluminum silicates.

PS

Hi can i get more details on this system as i am looking at a simlilar system.
 
Plasmasmelter, does the honeycomb have a higher melting temperature than the PGM that are attached to it??
Something of interest. A friend of mine had a number of samples of honeycomb assayed for all metals, and told me that not only were there PGMs present, but also large amounts of silver...
 