Gold Testing Solutions-
concentration for 333 kt gold: 2 parts nitric acid to 3 parts water
(distilled water)

concentration for 585 kt gold: pure concentrated nitric acid.

concentration for 750 kt gold: add a little amount of hydrochloric
acid to the concentrated nitric acid.

concentration for silver: 1 part of nitric acid to 3 parts of
hydrochloric acid (agua regia). This solution creates a white
deposite of silverchloride which turn into a dark violet color
depending on the amount of silver in your metalstrike used by a
touchstone procedure.If the metal doesn't contain any silver,the
metalstrike stay's gray or disapears after a while.
 
Didn't know where I should post this, but this looked like a good spot.
Purple gold on Ebay;

http://cgi.ebay.com/Purple-Gold-5g-ampoule_W0QQitemZ160107644401QQihZ006QQcategoryZ413QQrdZ1QQcmdZViewItem

It says it is 79% gold and 21% aluminum.
 