cleaned up some filters and such

Gold Refining Forum

Help Support Gold Refining Forum:

This site may earn a commission from merchant affiliate links, including eBay, Amazon, and others.

mlgdave

Well-known member
Joined
Feb 7, 2011
Messages
222
Location
Mariposa CA
was pale yellow Aucl, added SMB, nothing happened, i came back in this morning and will ya look at what I found! Whole inside of the jar had some incredibly thin (and fragile) gold leaf on it.

Im drying it now see how much weight!
jar.jpg

leaf.jpg


I dont imagine this is any strange phenomenon, I just thought it pretty cool.

mlgdave
 
it was 0.97 grams of gold, was pretty cool.

onto the next batch, boy I hope it stops snowing, I wanna run plumbing out to the shop now that im taking this on as a full time vocation!

Hoke is some AMAZING reading and has me more freaking excited than buying gold for 50%

mlgdave
 

Latest posts

Back
Top