I have started working on some silver lately and have been a bit surprised with some of the results. Here is a button (?) that I converted from silver chloride using iron and sulfuric acid. I done this as a test to see how difficult it might be and and to compare it with the lye/karo process. I am thinking I will stick with the iron/sulfuric process for now.