CPU gold content

Gold Refining Forum

Help Support Gold Refining Forum:

This site may earn a commission from merchant affiliate links, including eBay, Amazon, and others.

LaurenceOs

Well-known member
Joined
Jun 7, 2009
Messages
98
Location
Near London, England
A friend of my just gave me 5 pentium 3's and they look good but im just wonder which cpus are the creme, the real juicy *******s?

Also sid note, it appears that the gold pins are secured with silver? is that how it is?

Cheers chaps
 
The real "juicy's" (lol) in CPU land are #1 386's and 486's,#2 would be pentiums with top and bottom gold lids,then would have to be pentium pros.These are in order by weight not by the piece,and thats my guess,Im sure others will add what they think as well.
Johnny
 
Aren't most P3s like fiber P1s and celerons mostly made with Kovar which is ~52% iron, 29% nickel, 18% cobalt? The little discs where the pin attaches to the package is usually a nickel alloy of some sort.
 
I don't have the exact chemical composition in front of me,but right off hand that doesnt sound right.And even if I am wrong they are still CPU's that contain gold.If you have a bunch but don't think they are worth anything,or not worth processing,I can name 20 people on the forum that will gladly take them off your hands,matter of fact Jim is close enough to drive to you and pick them up if you had enough.......lol.
Johnny
 

Latest posts