Has anyone tried not diluting their pregnant AR solutions and just chill it instead?

The reason I ask is that I would prefer not to dilute the solution and just chill it as the quantity that I am refining is starting to increase, my limit is currently at 250g of refined gold.

I would like to do some tests myself but unfortunately there is no assay lab in my country who would accept small quantities of samples.
 