A arthur kierski Well-known member Joined Feb 10, 2008 Messages 1,119 Location são paulo---brazil Aug 3, 2020 #1 i have a powder (gold powder) that after dried ,burns spontaneosly--the powder was cenented with iron sponge-------what powder is mixed with the gold powder?thanks for answer
i have a powder (gold powder) that after dried ,burns spontaneosly--the powder was cenented with iron sponge-------what powder is mixed with the gold powder?thanks for answer
L Lou Moderator Staff member Moderator Joined Nov 4, 2007 Messages 5,239 Location Rhodia Drive Aug 3, 2020 #2 It's the iron. I'd put it all in 1:1 muriatic and water.
A arthur kierski Well-known member Joined Feb 10, 2008 Messages 1,119 Location são paulo---brazil Aug 3, 2020 #3 Dear Lou---thanks for the answer--- i am teachig my son,and i am kind of rusty----yours Arthur Kierski