filter paper

Gold Refining Forum

Help Support Gold Refining Forum:

This site may earn a commission from merchant affiliate links, including eBay, Amazon, and others.
for the gold refining process.
refining pins fingers with the acid peroxide method.
thanks
 
the guy at the shop told me the have many types and grades. he mention some like membrane, fiber,....no1, no2.
i dont know if i can get a normal coffee filter.
can i empty a tea bag and use that? just a thought :idea:
 
andees78 said:
the guy at the shop told me the have many types and grades. he mention some like membrane, fiber,....no1, no2.
i dont know if i can get a normal coffee filter.
can i empty a tea bag and use that? just a thought :idea:
Every food store carries coffee filters
 
wrecker45 said:
i can get nitric acid $ 56.95 canadian for 2.5 litres is this a good price
It's a matter of one's perspective. If you are properly connected, you should be able to buy nitric acid for a price in the neighborhood of $5/gallon. That, of course, is in bulk packaging, likely available (now) only to licensed operations. In the early 90's, I was paying $207 (American) for a 55 gallon drum.

Harold
 