Well after being away for a while due to work and another baby, I was finally able to get out into the shop and have at it again. Produced my biggest one so far.

As you all know I accept all angles of criticism. Let me have it lol.
 

Attachments

  • 20160420_163203.jpg
    20160420_163203.jpg
    2.2 MB
This one is 18.61. Most of it is from gold filled pocket watches, and very little from processed filter papers.

Thanks guys

Lol not big enough. . It always seems like that doesn't it? Always amazes me on how heavy they are for their size.
 
Thanks guys, this is only the 4th one I have ever done. Was pretty worried I might have forgot how to do it, but once I got going it all came back to me lol. Definitely looks better then my first 3
 