A
Anonymous
Guest
Here are some pictures, as perscribed by many I watched Steve's videos and read a bunch of hokes book, after taking in a fair amount of info. I put on my smelting shoes and went to work.
I know this is only step 1. But is is a step and none the less I am proud of the results.