I have to strip a quantity of these for a friend,they run at around 0.2% Au and I was aiming to strip them in a weak cyanide solution to recover the gold but I'm open to any better suggestions.
 
GSP I did consider the cell as Ive used one before but thought the cyanide might be easier and faster as there's 100 kilos plus of this stuff, and I'm used to using it!
 