I did search but couldn't find anything on this specific issue.
Ok I processed fingers in AR, washed them off and got all the foils. I cleaned these with boiling water and put them in AR. After filtering a nice golden liquid came out and I dropped with SMB. 24 hours later I siphoned off the liquid and allowed the last bit to air dry, woohoo gold! I decided to process this powder again to produce a more pure product and here is where the problem happened. Same process, AR, filter, neutralise, SMB and then I noticed the gold was sticking to the side of the beaker where I imagine there are tiny scratches.
I tried rinsing it off with boiling AR, but it's so pure it doesn't seem to dissolve and I'm stuck as to what I can do here. Any ideas?
Ok I processed fingers in AR, washed them off and got all the foils. I cleaned these with boiling water and put them in AR. After filtering a nice golden liquid came out and I dropped with SMB. 24 hours later I siphoned off the liquid and allowed the last bit to air dry, woohoo gold! I decided to process this powder again to produce a more pure product and here is where the problem happened. Same process, AR, filter, neutralise, SMB and then I noticed the gold was sticking to the side of the beaker where I imagine there are tiny scratches.
I tried rinsing it off with boiling AR, but it's so pure it doesn't seem to dissolve and I'm stuck as to what I can do here. Any ideas?