Hi folks
Have any of the folks here actually managed to process these and get any results? There's all kinds of theories about them and I'd be very interested in hearing from anyone who has managed to get any progress.
~Oh yes Kurt the fuzzies rock. I've got all those!Jon - there is not a lot of gold associated with the ceramic processors as there are no bond wires - just gold dots/pads on the under surface of the ceramic processor - VERY LOW yield
However - where the processor makes contact with the board there should be a plastic cage that has "fuzz buttons" in it which are relatively GOOD yield
Here is a trip down memory lane ----------
https://goldrefiningforum.com/threads/sun-ultra-sparc-cpus.16018/
What you show here is "a bit" different (multi-chip instead of single chip) so I am just "guessing " that because it is Sun Ultra Sparc ceramic technology the "fuzz button" connection is the same ?
Kurt