How do you cement the silver in AR that has gold and silver

Gold Refining Forum

Help Support Gold Refining Forum:

This site may earn a commission from merchant affiliate links, including eBay, Amazon, and others.

Refiner232121

Well-known member
Joined
Jul 4, 2009
Messages
177
I have a batch that is a like a stock pot
I don't know if I can call it that

This is left of chemicals from here and there
My question is this
If I have AR mixed with gold and silver in there plus other precious metals
Hoke talks about the platinum group and gold but how do you separate the silver from gold and the other metals
Hoke doesn't say anything about that.
How do you cement the silver in AR that has gold and silver
Do you use ice or something else
 
Barren Realms 007 said:
The HCL in your AR should turn the silver to silver chloride. Then you can process it once filtered as described on the forum.

Yup.



Refiner232121
There's a reason why she didn't addressed that.

While cold and dilute and with no oxidizers, your stock pot solution will not hold AgCl in it, it will precipitate it as fine white/gray powder in time.
Even hot, concentrated AR will not dissolve great amounts of silver, only traces and usually the fine silver particles.

You can not cement something that ain't there..., and don't forget about all of the other metals that are lower on the EMS that will co-cement as well.
 