Elemental Well-known member Supporting Member Joined Sep 17, 2020 Messages 196 Location Charlottesville, VA Dec 7, 2021 #2 Add copper metal to cement out the silver. Try not to have excess nitric in your solution as it will eat lots of copper.
Add copper metal to cement out the silver. Try not to have excess nitric in your solution as it will eat lots of copper.
FrugalRefiner Administrator Staff member Administrator Supporting Member Moderator Joined Jan 14, 2012 Messages 6,642 Location Ohio, USA Dec 7, 2021 #3 See When In Doubt, Cement It Out. Dave
L Lino1406 Well-known member Joined Nov 1, 2007 Messages 2,356 Location Israel Dec 8, 2021 #4 If you want a quicker drop, add to nitrate solution hydrogen peroxide, and then, carefully, a soda caustic solution. Start trial with low concentrations