zauggart Well-known member Joined Feb 11, 2008 Messages 68 Location fredericton nb canada Apr 6, 2008 #1 on ic's etc the outer pins lead to thin gold wire inside and i was wondering what is the karat of the thin wire is, does anybody know? thanks ian
on ic's etc the outer pins lead to thin gold wire inside and i was wondering what is the karat of the thin wire is, does anybody know? thanks ian
SapunovDmitry Well-known member Joined Dec 7, 2007 Messages 332 Location Moscow Apr 6, 2008 #2 Wires are almost always 100% gold, silver or Al.