I just bought this as SMB
It is French and the guy said it is SMB
I wanted to know if anyone can say it really is SMB
I will also have to search on how much water to mix with this white powder
Potassium metabisulfite (PMB) Is not the same like sodium metabifulfite (SMB) however, as far as I now they ar intechangeable !!!
You ca use potassium metabisulfite (PMB) same way you use SMB