Harold_V;  You are right of course, the sulfuric should be above 66% to penetrate the plate.  I stand corrected. 

I believe the extra oxidation from dichromates or some other oxidizer does help to promote flaking.  Glycerin coupled with caustic reduces platinum salts to metal (platinum black), but I've never understood why one would think it would help in a acidic stripping cell.  Dr. Poe