Is this Platin?

Gold Refining Forum

Help Support Gold Refining Forum:

This site may earn a commission from merchant affiliate links, including eBay, Amazon, and others.

leHAI

Active member
Supporting Member
Joined
Oct 7, 2024
Messages
35
Location
vietnam
Bros, please tell me is this Platin and how to get it from solution

I have materials which has gold so I put them to acid nitric solution to separate gold (picture 2)
I Test Stannous the solution and get the brown colour ( middle paper in picture 1)
 

Attachments

  • z6028775733632_148e15ac7c9153fb7a14119807c7db9c.jpg
    z6028775733632_148e15ac7c9153fb7a14119807c7db9c.jpg
    304.8 KB
  • z6028775741898_f30b6523a7de292a929bea9d35c1e420.jpg
    z6028775741898_f30b6523a7de292a929bea9d35c1e420.jpg
    391.5 KB
Bros, please tell me is this Platin and how to get it from solution

I have materials which has gold so I put them to acid nitric solution to separate gold (picture 2)
I Test Stannous the solution and get the brown colour ( middle paper in picture 1)
What material do you have?
Nitric do not dissolve Platinum nor Gold.
It do dissolve Palladium and Silver.
This color seem like one of the false positives.
 
If the connectors are magnetic, then there is nickel there.
at least the sublayer on which gold is applied.
Nickel does not dissolve in nitric acid, even with heating.
platinum and gold are a rare combination, these are just some kind of military connectors or gold-plated contacts from a relay.
 