Is this rhodium?

Gold Refining Forum

Help Support Gold Refining Forum:

This site may earn a commission from merchant affiliate links, including eBay, Amazon, and others.

hodhod1403

Member
Joined
Jun 10, 2024
Messages
22
Location
Iran
First, I dissolved the soil in AR and heated it
After an hour, sponge clouds were formed on the soil inside the AR, which was not dissolved. I separated them and washed them, then they did not dissolve in nitric. Is that rhodium?
 

Attachments

  • IMG_20241206_134944.jpg
    IMG_20241206_134944.jpg
    3 MB
First, I dissolved the soil in AR and heated it
After an hour, sponge clouds were formed on the soil inside the AR, which was not dissolved. I separated them and washed them, then they did not dissolve in nitric. Is that rhodium?
Please say this is not the same "Soil" you have been at all the time?

Do you have an Assay now?

The only answer I can give you with some substance to it is that your question can not be answered.
There is not enough data from you, not enough of anything other either for that matter.

Have you tried to cement out what you have on Copper?
 