S silversaddle1 Well-known member Joined Mar 19, 2008 Messages 1,563 Location Iowa May 13, 2010 #1 Did anybody ever come up with a basic number on these? I did a search and came up with nothing.
lazersteve Well-known member Moderator Emeritus Joined Feb 27, 2007 Messages 7,334 Location Florida May 13, 2010 #2 Try these threads: Keybaord Yields 1 and Keyboard Mylars There are other posts too, just use the search tool on my website. Steve
Try these threads: Keybaord Yields 1 and Keyboard Mylars There are other posts too, just use the search tool on my website. Steve
S silversaddle1 Well-known member Joined Mar 19, 2008 Messages 1,563 Location Iowa May 13, 2010 #3 Steve, Thanks! My search is never good! Scott
lazersteve Well-known member Moderator Emeritus Joined Feb 27, 2007 Messages 7,334 Location Florida May 13, 2010 #4 silversaddle1 said: Steve, Thanks! My search is never good! Scott Click to expand... Scott, Are you using the forum search tool on my website? Steve
silversaddle1 said: Steve, Thanks! My search is never good! Scott Click to expand... Scott, Are you using the forum search tool on my website? Steve
S silversaddle1 Well-known member Joined Mar 19, 2008 Messages 1,563 Location Iowa May 13, 2010 #5 Naw, just the search box on the top of this page.
Chumbawamba Well-known member Joined Jan 7, 2009 Messages 364 Location Gold Country, California Jul 17, 2010 #6 For the record, the typical yield seems to be 0.25ozt per pound, or 17g per kilogram. For more perspective, that's 1ozt of silver for every 4 pounds of mylars, or 500ozt per ton. Once I do a batch I'll of course post my results.
For the record, the typical yield seems to be 0.25ozt per pound, or 17g per kilogram. For more perspective, that's 1ozt of silver for every 4 pounds of mylars, or 500ozt per ton. Once I do a batch I'll of course post my results.