How to melt copper powder which is recovered from iron or Aluminium
tried different ways and flux?
Hrushi
tried different ways and flux?
Hrushi
It's not hard to melt. Simply fill a crucible, fire, then add flux when it's molten, or when the material is hot enough to liquefy the flux. If you choose to use anhydrous borax, or borax glass, even that's not a problem. It can be added when the charge is cold, because it's much heavier and doesn't get blown out of the crucible as easily.hrushi said:How to melt copper powder which is recovered from iron or Aluminium