Interesting Steve. Thanks. The DBC process felt lengthy and cumbersome to me. Almost prefer to dissolve twice, and precipitate once with SMB and once with oxalate, to obtain a very pure product but maybe not as good as with DBC. If it could be made simpler and faster, I'd like to learn about it.