My friend wants me to recover almost 200 lbs (pounds) of jewelry
I believe the bulk is gold plated brass which we have to by at brass scrap prices from the recycling yard so they will not be involved
He gave me about 55grams to see what I could do
What he gave me was 12k and 14k gold filled
Let's just say 55grams of 12k 1/20th
So 50% (27grams) is gold filled
1/5 of 27 is about 5 1/2 grams
Is this correct
And if I remember I think kdiver (sorry is misspelled) did an excellent video on gold filled
I will look for it
Thanks steyr223
Any tips or thoughts would be greatly appreciated
How is everyone
This is going to b good if my calculations are correct
My friend wants me to recover almost 200 lbs (pounds) of jewelry
I believe the bulk is gold plated brass which we have to by at brass scrap prices from the recycling yard so they will not be involved
He gave me about 55grams to see what I could do
What he gave me was 12k and 14k gold filled
Let's just say 55grams of 12k 1/20th
So 50% (27grams) is gold filled
1/5 of 27 is about 5 1/2 grams
Is this correct
And if I remember I think kdiver (sorry is misspelled) did an excellent video on gold filled
I will look for it
Thanks steyr223
Any tips or thoughts would be greatly appreciated