joekelly
Member
:?: My 1st attempt at gold recovery stopped in its tracks. I took a friends advice and tried 2 parts Muratic acid and 1 part Hydrogen Peroxide to extract gold from pc boards and cell phones. He has since went missing and I dont know what the remainder of this process is. I'm a single father so a cheap process is what I need. Currently I have cleaned and soaked alot of pieces. Cleaning out the bath of stripped parts, replacing them with more. Over and over in wait of my friends return. The solution is now black, speckled heavily with gold flakes/particles, it has thickened to the point said particles stay suspended, the bottom of bath container is covered with a very fine, white, glittery sand, and is considerably heavier. This is as far as i;ve gotten. Repeating this process and filling up bottles. Any instruction would be appriciated and recipricated, my current resources, as well as those to be aquired will be openly shared via this website. Any guesses what might be in this solution? Bottles filled with water weighed 20 oz. The same bottles filled with post bath solution range from 27-30 oz. Most components were from old Nokia and VioceStream cell phones. Thanks, joe