I am a chemist/materials scientist currently suffering the economic collapse of Michigan. I pulled a short term contract to extract palladium from precious metals slimes in a gold refinery. Very interesting. I just want to say thank you in advance for the information i have learned regarding palladium. It worked like a charm and the masters of precious metals are very impressed with my results.

As a result of all this, I have been checking out the gold markets etc and am now looking at my own extractions. So far, 3 ounces of gold and about 40 of silver turned over to the refinery.