Hello every one , i got this test result from a friend can any one tell me what type of test is this xrd or xrf ...etc , and what the circled word below indicates
 

Attachments

  • Screenshot_20230905-150900.jpg
    Screenshot_20230905-150900.jpg
    265.8 KB · Views: 1
It means the meter is not calibrated to gold but it's measurement is derived from other data in the device. What does your friend say about this? Does he have a manual?
 
Hello every one , i got this test result from a friend can any one tell me what type of test is this xrd or xrf ...etc , and what the circled word below indicates
As far as I see, there is no indication say what device is used.
Butvit do not look like the XRF I have seen.
Your friend might tell you more.
 