Mountain Man
Well-known member
- Joined
- Sep 11, 2016
- Messages
- 102
Fellow gold producers.
I have a situation that I am at a loss over and know with the vast knowledge that abides on this forum you will have the answer to my dilemma.
I have 3 jars of solution from A.R. recovery method. All three have been neutralized with urea and treated with sodium metabusulfite. I tested for gold before add the precipitant and all 3 show black and purple and not faintly but prominent.
The problem is the gold won't drop. So I tested again with s.chloride and again it shows heavy gold content in all 3 batches but still cannot get it to drop.
My theory is that the ph level is off but I have no way of testing that as of now.
Can I impose on your vast wealth of knowledge once again to guide in the right direction.
Thank you in advance.
I have a situation that I am at a loss over and know with the vast knowledge that abides on this forum you will have the answer to my dilemma.
I have 3 jars of solution from A.R. recovery method. All three have been neutralized with urea and treated with sodium metabusulfite. I tested for gold before add the precipitant and all 3 show black and purple and not faintly but prominent.
The problem is the gold won't drop. So I tested again with s.chloride and again it shows heavy gold content in all 3 batches but still cannot get it to drop.
My theory is that the ph level is off but I have no way of testing that as of now.
Can I impose on your vast wealth of knowledge once again to guide in the right direction.
Thank you in advance.