May i ask if these power connectors found in printers, power supply and etc. is silver or just some kind of metal ?
 

Attachments

  • DSC00105.JPG
    DSC00105.JPG
    145.3 KB · Views: 446
have you tested the lpug to see if it contains anything /silver,ext ,i dont think they do ,anyone else!!!you can find how to test it in this forum,good luck
 
Pull the pins and put them in your brass scrap. Only the parts that handle the digital data signals might contain values. Power cords, power connectors, ground straps are base metal scrap.
 