Precipitation and turning 2 metallic silver

Gold Refining Forum

Help Support Gold Refining Forum:

This site may earn a commission from merchant affiliate links, including eBay, Amazon, and others.

Rickard3585

New member
Joined
Jul 13, 2021
Messages
3
So I question never done this before I've done it with dry sodium hydroxide but not with liquid I have silver chloride and I need to turn it into metallic state I have liquid sodium hydroxide from the lab wondering if I could use that along with sugar to turn it into a metallic
 
Back
Top