mohamedmsud
Member
- Joined
- Nov 9, 2018
- Messages
- 16
Hello my friends
After a great deal of trouble, I was able to use Aqua Riga on soil . This was done very successfully. The results were impressive. The samples were from 1 kg to 5 kg. The problem that is now facing me is in the filtration. I used to extract the solution using filter paper and cotton.
Now I have decided to work in large quantities to expand the project, any suggestions for filtering, with larger quantities.
thank alot
After a great deal of trouble, I was able to use Aqua Riga on soil . This was done very successfully. The results were impressive. The samples were from 1 kg to 5 kg. The problem that is now facing me is in the filtration. I used to extract the solution using filter paper and cotton.
Now I have decided to work in large quantities to expand the project, any suggestions for filtering, with larger quantities.
thank alot