Anybody of you used www.propertyroom.com to buy scrap solid gold??
If yes, what was your experience?
It is the best I could find after I started my personal war with EBay (well they started it w me).
I just recieved today my first lot. It was a small lot of 5 grams of 10karats gold.
Well half of it was fake. I already sent them an email.
They claim that they test the gold but I think they don't or if they test it they do it wrong
I'm quite confident about my testing capabilities. I use an electronic tester. I tested over 50k$ worth of gold in the last 4 months and the results from the refinery were always around what I expected with a marginal error of less than 1%. So if I was expecting 5000$ from the refinery it was either 5050$ or 4950$.
I still have some small 14karats order to come in from the www.propertyroom, I will let you how that look.
Any other suggestion about where to buy gold solid scrap that is not EBay?
Filippo
If yes, what was your experience?
It is the best I could find after I started my personal war with EBay (well they started it w me).
I just recieved today my first lot. It was a small lot of 5 grams of 10karats gold.
Well half of it was fake. I already sent them an email.
They claim that they test the gold but I think they don't or if they test it they do it wrong
I'm quite confident about my testing capabilities. I use an electronic tester. I tested over 50k$ worth of gold in the last 4 months and the results from the refinery were always around what I expected with a marginal error of less than 1%. So if I was expecting 5000$ from the refinery it was either 5050$ or 4950$.
I still have some small 14karats order to come in from the www.propertyroom, I will let you how that look.
Any other suggestion about where to buy gold solid scrap that is not EBay?
Filippo