Hello everybody,
Someone knows if this kind of relays contains PM? I ask because they look not not easy to remove without heatgun. thank you, have a good day!
I stumbled across some of these. Not exactly these ones, but similar. Mine were easy to remove from inside.
Contact points inside the tube are often plated with precious metals.
Mine were rhodium plated. Need to be tested
Thanks @BlackLabel , Yes, I did it, I put a couple of them in HCl to dissolve the Fe-Ni 50:50 alloy of the main body. It looks more acid-resistant than I thought