kjavanb123
Well-known member
Hi all,
I know this site mostly talk about gold and precious metals refining. I am curios in order to produce the pure saleble ferroalloy from ferroalloy concentrate, what type of furnace would be the best? In one of our project, we produce 2tons of 80% ferromanganese concentrate daily, which needs to be remelted to produce the 99% Ferromanganese. Any suggestions? Happy New Yr
I know this site mostly talk about gold and precious metals refining. I am curios in order to produce the pure saleble ferroalloy from ferroalloy concentrate, what type of furnace would be the best? In one of our project, we produce 2tons of 80% ferromanganese concentrate daily, which needs to be remelted to produce the 99% Ferromanganese. Any suggestions? Happy New Yr