I have heard of a simple processs for refiinf silver chloride using sulphuric acid and iron-anyone know it or tried it? Also has anyone tried the sucrose method using silver oxide? Results? suggestions? Thanks
The sulfuric and iron works but you need to add distilled water to the mix. And the sodium hydroxide and sucrose works as well. But you are supposed to be processing silver chloride in these 2 processes.