Dear friends of the forum:

Please, I would like to know if I am right with these formula:


    3 Ag2S + 8 HNO3 = 6 AgNO3 + 4 H2O + 2 NO + 3 S


    AgNO3 + ClH = ClAg + NO3H

My goal is to re use the nitric acid used in the first step of the reaction.

Could it be possible ?

With my best regards

Luigi