Ibex
Member
Anybody has idea about this formula?
product name: Rhodium (III) Sulfate solution (liquid) bright plating precious metals solution *
* ~ 8% in H2O
origin: 100% made in European Union * (according to ECHA-REACH)
purity:> 99.00% min. (raw virgin matter, extra pure, selected)
quality level: 100
C.A.S. number: 10489-46-0
MDL: MFCD00016309
EINECS: 234-014-5
NACRES: NA.23
linear formula: Rh2 (SO4) 3
molecular formula: O12Rh2S3
pubChem substance ID: 24864741
NACRES: NA 23
formula weight: 494.00
density: 1.217 g / mL at 25 ° C (lit.)
vapor pressure: <= 1100 hPa @ 50 ° C
specific gravity: 1.4 g / cm
solubility: miscible with water, ethanol and with a 3: 1 ethanol / water mixture
storage & sensitivity: ambient termperaturee
assay (unspecified):> 99.00 +%
assay (unspecified): Rh 4.00-6.00%
form: liquid
product name: Rhodium (III) Sulfate solution (liquid) bright plating precious metals solution *
* ~ 8% in H2O
origin: 100% made in European Union * (according to ECHA-REACH)
purity:> 99.00% min. (raw virgin matter, extra pure, selected)
quality level: 100
C.A.S. number: 10489-46-0
MDL: MFCD00016309
EINECS: 234-014-5
NACRES: NA.23
linear formula: Rh2 (SO4) 3
molecular formula: O12Rh2S3
pubChem substance ID: 24864741
NACRES: NA 23
formula weight: 494.00
density: 1.217 g / mL at 25 ° C (lit.)
vapor pressure: <= 1100 hPa @ 50 ° C
specific gravity: 1.4 g / cm
solubility: miscible with water, ethanol and with a 3: 1 ethanol / water mixture
storage & sensitivity: ambient termperaturee
assay (unspecified):> 99.00 +%
assay (unspecified): Rh 4.00-6.00%
form: liquid