Hello everyone, new here and making fierst stept in to gold refining world.

I would like to know if any of the above that i mentioned contain a fair amount of gold or they don't worth to buther. ?

i done some search here about that and came up eamty...

Thank you all
 
they do contain gold, the question is what one consider as fair amount of gold. i personally never throw away anything from mentioned above if there is visible gold on them. small drops make a river.
 
thank you for your answer.

do you know if all three of them can be treated as hole with AP and then acid-clorox ?

maybe different base metals... i do not know..

thanks again.
 
on sd card and sim card I would cut part with fingers and that will be candidate for AP.
as for usb I think that this is rather different as they are basically plated pins so another method will be probably better - like cell with copper mesh basket for deplating pins. check lazersteves webpage you can see this cell in action there.
 