I recently started refining from electronic scrap with the shor kit liquid turned dark emerald green no gold dropped test solution light brown for gold in solution then they told me to put tin in it and the sludge dropped to the bottom cleaned with ammonia the distilled water 3 times till tested clear dried to powder but it's not brown it's more dark green
 
jimdoc said:
Not again.....................


:eek: I'm afraid it looks the same from this side too.

I recently started refining from electronic scrap with the shor kit liquid turned dark emerald green no gold dropped test solution light brown for gold in solution then they told me to put tin in it and the sludge dropped to the bottom cleaned with ammonia the distilled water 3 times till tested clear dried to powder but it's not brown it's more dark green

What was Shor's reply to your request for help?
 
Looks like another victim. Very glad I never placed an order with them.

Good news, though. There are a few members here that are familiar with Shor that may be able to help.

Time for more coffee.
 
Green would be copper.
If you haven't melted it yet and it's still in powder form rinse it a couple of times with warm hcl, rinse a couple of times with cold water and see what it looks like.
 