Silver cell 4?

Gold Refining Forum

Help Support Gold Refining Forum:

This site may earn a commission from merchant affiliate links, including eBay, Amazon, and others.
48 hours 47 minutes in action
Entire beaker slightly greenish tint
Anode basket 3/4 full
Good silver growth on the edges
Seems like Silver particles in solution
 

Attachments

  • IMG_8891.jpeg
    IMG_8891.jpeg
    1.6 MB · Views: 1
  • IMG_8890.jpeg
    IMG_8890.jpeg
    1.3 MB · Views: 1
Last edited:
Day four (the stop watch function quit )
Solution same color
Conductivity .3 A/1. VDC
Crystals had to be knocked down today
Trr
 

Attachments

  • IMG_8919.jpeg
    IMG_8919.jpeg
    1.7 MB · Views: 0
Had to shut it last night
Slimes dropped on the crystals twice
Looks like the plastic coating on the wire started to deteriorate .
Cleaning up , cementing 1/2 the electrolyte out
Cement silver looks great
Probably the last time using the graphite anode
 

Attachments

  • IMG_8932.jpeg
    IMG_8932.jpeg
    1.5 MB · Views: 0
  • IMG_8928.jpeg
    IMG_8928.jpeg
    1.6 MB · Views: 0
Cement silver from half the electrolyte
Left pictures is from cement silver less then 24 hours much cleaner
Right was left in for a week , more copper in the silver cement
 

Attachments

  • IMG_9078.jpeg
    IMG_9078.jpeg
    1.8 MB · Views: 0
  • IMG_9076.jpeg
    IMG_9076.jpeg
    1.2 MB · Views: 0
Lessons learned
Time for stainless steel bowl
new crucible (ordered )
Found lead and tin in one sample
99.43/ 97/94
Didn’t keep track of the ugly bars when melting into bigger bar drag
 

Attachments

  • IMG_9043.jpeg
    IMG_9043.jpeg
    2 MB · Views: 0
  • IMG_9152.jpeg
    IMG_9152.jpeg
    2 MB · Views: 0
  • IMG_9150.jpeg
    IMG_9150.jpeg
    1.4 MB · Views: 0