When I charge Refinery Mud (obtained from lead electrorefining) in Noble furnace for reduction dust is collected in bag filters.This dust contains antimony ranging from 50-58% and silver from 1.5-2%.We are generating 20 tons of antimony dust on a monthly basis so effectively we are losing 300-400 Kg of silver.Is there any means to recover it?
 
Please give the description of stages in getting Sb dust, from raw material, source, including temperatures. What the rest of 42% besides antimony?
 