hey just a quickkie , sim cards look like they have gold on um is this the case?, thanxs for those who take time to reply,kev
 
Hi Kev,

I guess you could but you would need hundreds of them to make it anywhere near worthwhile.

The plating on them is very very thin.

Buzz
 
chears buzz,i carnt wait to do my first run a bit away yet tho, so simcards are ok to cut rd the gold bits and chuck them in there also with the rest ov the stuff, also i took apart a fruit machine and tryed to get pics up ov the boards cuz dont look like anygold just all silver or solder i guess , but i hear the chips have gold inside is this only sum chips or all? chears agin
 
I'm not sure. The most I ever did was 300. Much of the gold got dissolved and went into another AP batch so I didn't get yield data. The surface area of gold on the sim cards varies widely.

I would love to have a pile of them. They strip really clean. :)
 
Recycle.net has them priced at $16-32/pound. I don't know what they base their prices on, some of them seem really bizarre.

As with most good e-scrap, your'e probably looking at a few grams per pound tops. 1000 sims is probably only a few ounces. Lot's of speculation here, don't base your decisions on my fuzzy math.
 
Ive processes 10 or so '3G' ones and they seemed to be nicely plated as they completely stripped off in nice foils in AP. It wasn't enough for me to do a yield or anythign and the foils just went into a pile with others.
In the middle of the gold plating, one of the foils looks kinda like a golden cat converter haha

Also, Ive been gettign toner contacts from printers from my work lately. Not a lot but each one has 2 half square inch gold contacts and they also strip nicely in AP.
 