Some recent buttons / bars

Gold Refining Forum

Help Support Gold Refining Forum:

This site may earn a commission from merchant affiliate links, including eBay, Amazon, and others.

joekbit

Well-known member
Joined
Oct 10, 2014
Messages
238
Just a few of the things I've been doing. #1 nice little bar, I think that one was 39 grams. #2 a funny looking quater, darn thing is heavy, 33 grams. Just found it in my pocket with the rest of my change. #3, 6 grams I set a dime on top of the button and hit it with a hammer
 

Attachments

  • IMG_1698(1).jpg
    IMG_1698(1).jpg
    763.5 KB · Views: 26
  • 20211123_140045.jpg
    20211123_140045.jpg
    1.4 MB · Views: 25
  • 20211203_123116.jpg
    20211203_123116.jpg
    1.1 MB · Views: 26