so then people can i add most things to this so called ap, like phones ,boards,sims, with out cutting the just gold bits off or as close as i can get
 
it wont blow up or nuffin will it if i addded batterys , plastics and wot not, anyone got a list of dos and donts i can look over, thank you, kev
 
Isolate high yield items. Fingers, ceramic cpu's, flat packs, pins.

By all means keep out aluminum and steel.

Garbage in, garbage out.
 